Ferrit RM Çekirdekleri

Ferrit RM Çekirdekleri

 

product-553-317
product-553-317

Modeli

G.W

BOYUT (mm)

A1

A

B

C

D

E

F

Gmin (İngilizce)

H

6 TL

5.6

14.4±0.3

17.55±0.35

12.65±0.25

8.0±0.2

6.3±0.1

4.1±0.1

8.8±0.1

8.8

10.3±0.3

8 TL

13.6

19.3±0.4

22.7±0.5

17.3±0.3

10.7±0.3

8.4±0.2

5.5±0.1

11.4±0.5

9.5

14.3±0.3

10 RM

24

24.1±0.6

27.8±0.7

21.6±0.5

13.2±0.3

10.7±0.2

6.3±0.2

9.3±0.1

10.9

16.2±0.3

12 RM

49

29.2±0.6

36.7±0.7

25.5±0.5

15.8±0.3

12.6±0.2

8.5±0.2

11.85±0.1

16.8

21.6±0.3

14 ₺

77

34.1±0.6

41.5±0.7

29.6±0.6

18.7±0.3

14.7±0.3

10.6±0.1

15.5±0.1

17.0

27.0±0.3

 

MODELİ

PARAMETRE

AL±25%(nH/N^2)

N.W(g)

C1mm (C1mm)-1

Lem

Aemm Belediyesi2

Zehir3

ZP40 Serisi

ZH7K Serisi

ZH10K Serisi

6 TL

0.784

29.2

37.0

1090.0

2150

6000

8600

4.9

8 TL

0.604

38.4

63.0

2440.0

3300

8750

12500

12.0

10 RM

0.462

44.6

96.6

43100.0

4000

11200

16000

22.0

12 RM

0.388

56.6

146.0

8340.0

5000

13000

17700

45.0

14 ₺

0.35

70

198.0

13900.0

5700

14500

19600

67.0