Ferrit EE Çekirdekleri

Ferrit EE Çekirdekleri

product-438-285

 

MODELİ Brüt ağırlık

Boyut(mm)

A

Bmin (Türkçe)

C

D

E

F

EEL27

33

27.0±0.6

19.0 dk.

7.8±0.25

10.5±0.3

11.5±0.25

15.5±0.25

EE28 Serisi

24

28.0±0.6

18.6

7.2±0.2

10.7±0.3

6.5±0.3

10.5±0.3

EE28.5

23

28.8±0.6

21.1

7.2±0.2

10.4±0.2

6.5±0.3

10.5±0.3

EE30/7

24

30.0±0.5

19.9±0.4

6.9±0.3

7.1±0.2

10.0±0.2

15.0±0.2

EE32/9.5

36

32.1±0.5

22.7

9.5±0.3

9.5±0.2

11.5±0.3

16.4±0.2

EE32/11

42

32.1±0.5

22.7

9.5±0.3

11.0±0.2

11.5±0.3

16.4±0.2

EE32.6/37/9.5

40

32.6±0.5

23.6

9.5±0.3

9.5±0.2

14.3±0.3

18.6±0.3

EE33A

42

34.0±0.5

24

9.6±0.3

12.7±0.3

9.8±0.3

14.1±0.3

EE35/18

45

35.0±0.6

24.6

10.0±0.3

10.0±0.3

12.5±0.3

17.5±0.3

EE35/28

33

34.2±0.6

24

9.5±0.3

10.0±0.3

9.2±0.3

13.7±0.3

EE42/15/21

93

42.1±0.9

29.5

12.0±0.3

15.0±0.3

15.2±0.4

21.1±0.3

EE42/20/21

121

42.1±0.9

29.5

12.0±0.3

19.7±0.4

15.2±0.4

21.1±0.3

EE42/15/50

108

42.1±0.9

29.5

12.0±0.3

15.0±0.3

19.0±0.4

25.0±0.3

EE50 Serisi

120

50.0±0.7

34.2

14.6±0.4

14.6±0.4

13.1±0.3

21.5±0.3

EE55A Serisi

186

55.1±1.1

37.5

17.0±0.3

16.9±0.3

18.8±0.3

27.5±0.3

EE55B

230

55.1±1.1

37.5

17.0±0.3

20.7±0.3

18.8±0.3

27.5±0.3

EE55C

272

55.1±1.1

37.5

17.0±0.3

24.7±0.3

18.8±0.3

27.5±0.3

EE65A Serisi

304

65.2±1.3

44.2

19.6±0.3

19.6±0.3

22.5±0.3

32.5±0.3

EE65B

416

65.2±1.3

44.2

19.6±0.3

27.0±0.3

22.5±0.3

32.5±0.3

EE70A Serisi

412

70.5±1.5

48.0

16.7±0.5

24.5±0.6

24.6±0.6

35.5±0.5

EE70B

530

70.7±1.5

48.0

21.5±0.5

30.5±0.6

22.0±0.6

32.0±0.4

EE70/72

418

70.0±1.5

48.0

16.7±0.5

24.5±0.6

27.0±0.6

36.3±0.4

EE73/70

570

73.0±1.5

50.0

21.5±0.5

30.5±0.6

24.3±0.6

35.0±0.4

EE80/38/20

396

80.7±2.0

59.1

20.0±0.5

20.0±0.6

28.0±0.5

38.0±0.5

EE85A Serisi

726

85.0±3.0

55.0

27.0±0.4

26.5±0.5

29.0±0.5

44.0±1.0

EE85B

860

85.0±3.0

55.0

27.0±0.4

31.5±0.5

29.0±0.5

44.0±1.0

EE100 Dersi

1173

100.0+3.0/-1.5

72.0dk

28.0±0.5

28.0±0.5

46.0±0.5

60.0±0.5

EE110 Dersi

1700

110.0±3.0

74.2

36.0±1.0

36.0±1.0

38.7±0.6

57.0±0.5

EE130 Dersi

2410

130.0±3.0

89.0

40.0±2.0

40.0±1.0

43.0±0.8

63.0±1.0

EE160 Dersi

3400

160.0±3.0

120.0

40.0±2.0

20.0±1.5

64.0±1.0

83.0±1.0

EE188 Dersi

6880

185.0±3.5

128.0

55.5±2.5

55.0±2.0

49.0±1.5

79.0±1.5

EE193 Dersi

6880

193.0±3.5

132.0

58.0±2.0

59.0±2.0

49.0±1.5

79.0±1.5

EE210 Dersi

5620

210.0±3.5

149.0

58.0±2.0

40.0±1.0

65.0±1.5

95.0±1.5

EE240 Tezli Sistem

7000

240.0±4.0

176.0

56.0±3.0

40.0±1.5

86.5±1.0

117.0±1.0

 

 

MODELİ

Şartname

AL±25%(nH/N^2)

NET AĞIRLIK(g)

C1mm (C1mm)-1

Lemm (Türkçe)

Aemm Belediyesi2

Zehir3

ZP40 Serisi

ZH5K Serisi

ZH7K Serisi

ZH10K Serisi

CEEL27

0.867

70.0

80.7

5650.0

2500

27.0

EE28 Serisi

0.620

51.7

82.9

4290.0

3500

21.6

EE28.5

0.660

51.4

77.6

4000.0

3300

21.0

EE30 Serisi

1.089

65.4

60.0

3920.0

1980

19.4

EE32/9.5

0.890

74.6

86.3

6440.0

2500

32.0

EE32/11

0.746

74.6

100.0

7450.0

2900

37.5

EE32.6/37/9.5

1.026

85.5

83.0

7150.0

2200

36.0

EE33A

0.589

67.4

114.0

7690.0

3700

39.0

EE35/18

0.810

80.7

100.0

8070.0

2700

41.0

EE35/28

0.753

67.7

89.9

6090.0

2900

30.0

EE42 Dersi

0.534

97.0

182.0

17600.0

4700

86.0

EE42A

0.415

97.4

235.0

22900.0

6100

115.0

EE42/15/50

0.630

113.0

179.0

20227.0

3400

100.0

EE50 Serisi

0.425

95.8

226.0

21600.0

6100

115.0

EE55A Serisi

0.432

123.0

285.0

35050.0

5000

168.0

EE55B

0.348

123.0

354.0

43700.0

6500

220.0

EE55C

0.292

123.0

422.0

52130.0

7200

260.0

EE65A Serisi

0.373

146.8

393.1

57728.4

5800

280.0

EE65B

0.274

147.0

535.0

78700.0

7800

380.0

EE70 Serisi

0.344

159.0

409.0

73200.0

6500

380.0

EE70B

0.226

150.0

665.0

99800.0

9000

500.0

EE70/72

0.360

161.0

409.0

65800.0

10000

388.0

EE73/70

0.236

159.0

665.0

106000.0

9000

560.0

EE80/38/20

0.469

184.0

392.0

72300.0

6000

360.0

EE85A Serisi

0.264

188.0

714.0

134000.0

8300

660.0

EE85B

0.220

189.0

859.0

162000.0

10000

750.0

EE100 Dersi

0.344

270.000

784.000

222656.0

7300

1060.0

EE110 Dersi

0.191

244.0

1280.0

312000.0

11000

1520.0

EE130 Dersi

0.352

284.0

1600.0

454000.0

12000

2190.0

EE160 Dersi

0.498

398.0

1600.0

637000.0

9000

2500.0

EE188 Dersi

0.100

370.0

2940.0

1087800.0

21000

5700.0

EE193 Dersi

0.100

380.0

3580.0

1360400.0

21000

5800.0

EE210 Dersi

0.183

440.0

2400.0

1128000.0

13500

5400.0

EE240 Tezli Sistem

0.235

556.4

2359.0

1312421.0

12500

5900.0

Popüler Etiketler: ferrit ee çekirdekleri, Çin ferrit ee çekirdekleri üreticileri, tedarikçiler, fabrika

Soruşturma göndermek

(0/10)

clearall