FERRİT EPC ÇEKİRDEKLERİ

FERRİT EPC ÇEKİRDEKLERİ

product-351-290

 

MODELİ

G.W

BOYUT (mm)

A

Bmin (Türkçe)

C

D

E

F

G

Hmin

EPC13 Serisi

2.5

13.3±0.3

8.3

5.6±0.2

4.6±0.2

4.5±0.2

6.6±0.2

2.1±0.1

10.5

EPC17.8 Serisi

5.6

17.8±0.4

11.5

7.4±0.2

6.0±0.2

6.0±0.2

8.7±0.2

2.8±0.1

14.3

EPC34 Serisi

62

34.0±0.5

19.7

14.5±0.2

14.5±0.2

16.4±0.2

20.9±0.2

9.1±0.2

24.8

EPC39 Serisi

78

39.0±0.7

24.7

17.6±0.3

15.5±0.2

14.1±0.3

19.6±0.2

9.7±0.1

30.5

EPC41 Serisi

108

41.0±0.6

23.6

18.5±0.2

16.5±0.2

18.9±0.2

24.5±0.2

11.0±0.2

28.8

 

MODELİ

PARAMETRE

AL±25%(nH/N^2)

N.W(g)

C1mm (C1mm)-1

Lem

Aemm Belediyesi2

Vemm3

ZP40 Serisi

EPC13

2.46

30.6

12.5

382.0

870

2.1

EPC17.8

1.77

40.2

22.7

917.0

1200

4.5

EPC34 Serisi

0.73

89.6

122.6

10985.0

3200

56.0

EPC39 Serisi

0.60

87.95

147.0

12960.0

3700

70.5

EPC41 Serisi

0.57

104.1

183.2

19064.0

4100

97.0

Popüler Etiketler: ferrit epc çekirdekleri, Çin ferrit epc çekirdekleri üreticileri, tedarikçiler, fabrika

Soruşturma göndermek

(0/10)

clearall